Atik | Dyamèt (mm) | |||
0.05<=d<=0.09 | 0.09 | 0.25 | 0.50 | |
Tolerans (mm) | ±0.002 | ±0.003 | ±0.004 | ±d% |
Rezistans (Ωmm2/m) | <=0.017241 (Mou) | |||
<=0.01796 (Difisil) | ||||
Elongasyon (%) | >=13 | >=18 | >=20 | >=25 |
Fòs tansyon (MPa) | Mou:>=196; Di:350 | |||
Epesè kouch (um) | 0.3-10.0um | |||
Aparans | Pa gen reyur, tach lwil, kwiv ekspoze, oksidasyon, elatriye. | |||
Anbalaj | 5 pous, 8 pous, 9 pous, Kalite 300, Kalite 400, elatriye. | |||
Remak | Selon kondisyon kliyan yo |
SFil kwiv plake ajan
Atik | Dyamèt (mm) | ||
0.05<=d<=0.09 | 0.09 | 0.25 | |
Tolerans (mm) | ±0.003 | ±0.004 | ±0.005 |
Rezistans (Ωmm2/m) | <=0.01851 | <=0.01802 | <=0.0177 |
Elongasyon (%) | >=6 | >=12 | >=15 |
Fòs tansyon (MPa) | >=196 | ||
Epesè kouch (um) | 0.3-2.0 | ||
Strand | 7-100 | ||
Direksyon tòsyon an | Z (agoch) oubyen S (adwat) | ||
Longè kouche (mm) | 2.0-100 | ||
Aparans | Pa gen reyur, tach lwil, kwiv ekspoze, oksidasyon, elatriye. | ||
Anbalaj | Kalite 200, Kalite 300, Kalite 400, elatriye. | ||
Remak | Selon kondisyon kliyan yo |