Permalloy E11c Ni79Mo4 79HM mou fil mayetik alyaj

Deskripsyon kout:


Permalloy 80 se yon alyaj nikèl, fè ak molybdène. Li se yon alyaj mou mayetik ak pèmeyabilite mayetik eksepsyonèlman wo. Alyaj la gen yon coercivity ki ba, toupre zewo magnetostriction, ak siyifikatif magnetoresistance anisotropic. Magnetostriction ki ba a se kritik pou aplikasyon endistriyèl,

kote estrès varyab nan fim mens ta lakòz yon gwo varyasyon nan pwopriyete mayetik.


  • Modèl NO:Permalloy
  • Rezistans:0.55
  • Elongasyon (≥%):15-25
  • Klas:E11C
  • Ni:78.5-80.0%
  • Karakteristik:Segondè pèmeyabilite inisyal
  • Orijin:Lachin
  • Pwodwi detay

    FAQ

    Tags pwodwi

    Paramèt

    TABLE 1 Egzijans Chimik

    Eelement C≤ P≤ S≤ Mn Si Cu≤ Mo Ni Fe
    Konpozisyon% 0.03 0.02 0.02 0.6-1.1 0.3-0.5 0.20 3.8-4.1 78.5-80.0 Rès

    Nòt:

    Fòm ak dimansyon alyaj yo an konfòmite ak GBn198-88

    TABLE 2 Egzijans Fizik

    Pwopriyete Rezizivite (μΩM) Desinty (g/cm3) Curie Point.C Segondè saturation magneto-striksyon coefficientλθ/10-6
    Valè 0.55 8.6 450 2

    TABLE 3 Pwopriyete mayetik CA pou teren (valè min)

    Epesè Pik pou fòs chan mayetik la se 0.1A/m, Anba diferan frekans pèmeyabilite mayetik fleksib μm/(mH/m)
    60Hz 400Hz 1KHz 10KHz
    0.02 17.5 12.5
    0.05 18.8 9.4
    0.10 22.5 15
    0.20 12.5 7.5
    0.35 25 8.8

    TABLE 4 Koefisyan ekspansyon lineyè nan diferan Tanperati/(x10-6)

    Tanp 20-100 °C 20-200ºC 20-300ºC 20-400ºC 20-500ºC 20-600ºC 20-700ºC
    Valè 1.3-10.8 10.9-11.2 14.4-12.9 11.9-12.5 12.3-13.2 12.7-13.4 13.1-13.6

    TABLE 5 Egzijans mayetik (frèt woule teren)

    Klas I

    (δ&D)/mm μ0.08/(mHm)≥ μm (mHm) ≥ Bs/T≥ Hc(A/M)≤
    0.005 12.5 44.0 0.75 6.4
    0.01 17.5 87.5 0.75 4.8
    0.02-0.04 20.0 112.5 0.75 4.0
    0.05-0.09 22.5 137.5 0.75 2.8
    0.10-0.19 25.0 162.5 0.75 2.0
    0.20-0.34 28.0 225.0 0.75 1.6
    0.35-1.00 30.0 250.0 0.75 1.2
    1.10-2.50 27.5 225.0 0.75 1.6
    2.50-3.00 26.3 187.5 0.75 2.0

    Klas II

    (δ&D)/mm μ0.08/(mHm)≥ μm (mHm) ≥ Bs/T≥ Hc(A/M)≤
    0.02-0.04 22.5 125.0 0.75 2.4
    0.05-0.09 25.0 150.0 0.75 2.0
    0.10-0.19 27.5 187.5 0.75 1.6
    0.20-0.34 31.3 250.0 0.75 1.2
    0.35 32.5 275.0 0.75 0.79

    Klas III

    (δ&D)/mm μ0.08/(mHm)≥ μm (mHm) ≥ Bs/T≥ Hc(A/M)≤
    0.01 25.0 150.0 0.73 2.4
    0.02-0.04 31.0 190.0 0.73 1.6
    0.05-0.09 38.0 250.0 0.73 1.2
    0.10-0.19 38.0 250.0 0.73 1.2
    0.20-0.34 38.0 280.0 0.73 1.0
    0.35 44.0 310.0 0.73 1.0

    Hot Rolling(forge) Flastspring

    (δ&D)/mm μ0.08/(mHm)≥ μm (mHm) ≥ Bs/T≥ Hc(A/M)≤
    3-22 25.0 125 0.75 2.4

    Hot Rolling (Forge) Bar

    (δ&D)/mm μ0.08/(mHm)≥ μm (mHm) ≥ Bs/T≥ Hc(A/M)≤
    8-100 25.0 125.0 0.75 2.4